| Industry | Applications |
| Polymer Materials | Glass transition, melting behavior, crystallization analysis |
| Plastics & Rubber | Thermal stability, curing analysis, material comparison |
| Pharmaceuticals | Drug stability and thermal property evaluation |
| Chemical Industry | Phase transition and reaction analysis |
| Battery Materials | Thermal behavior and stability research |
| Food Industry | Ingredient thermal characteristics analysis |
| Research Institutes | Material development and scientific research |
| Quality Control Laboratories | Product consistency and performance testing |
| Parameter | Specification |
| Instrument Model | DZ-DSC300C Differential Scanning Calorimeter |
| Temperature Range | -40~600℃ |
| Temperature Resolution | 0.01℃ |
| Temperature Fluctuation | ±0.01℃ |
| Heating Rate | 0.1~100℃/min |
| Cooling Rate | 0.1~40℃/min |
| Constant Temperature Time | User adjustable |
| Temperature Control Mode | Automatic heating, constant temperature, cooling program control |
| Scanning Mode | Heating scan, cooling scan |
| DSC Measurement Range | 0~±600mW |
| DSC Resolution | 0.01μW |
| DSC Accuracy | 0.001mW |
| Gas Atmosphere Control | Automatic switching of two gas channels |
| Protective Gas Input | Available |
| Gas Flow Range | 0~300mL/min |
| Gas Pressure | ≤5MPa |
| Program Control | Six-stage heating and holding control |
| Display | 24-bit color 7-inch LCD touchscreen |
| Communication Interface | Standard USB |
| Calibration Standard | Indium, Tin, Lead |
| Power Supply | AC220V/50Hz (customizable) |
| Feature | DZ-DSC300C DSC Analyzer | Traditional Thermal Analyzer |
| Measurement Principle | Differential heat flow measurement | Usually single temperature measurement |
| Thermal Transition Analysis | Supports melting, crystallization, Tg, OIT | Limited functions |
| Temperature Control | Automatic multi-stage program control | Manual or basic control |
| Operation Interface | 7-inch touchscreen | Traditional buttons/software |
| Gas Atmosphere Control | Automatic dual gas switching | Manual adjustment required |
| Data Communication | USB interface | Limited connectivity |
| Calibration | User self-calibration supported | Usually requires professional calibration |